dc.contributor.authorMabuwa, Sipokazien_US
dc.contributor.authorMsomi, Velaphien_US
dc.contributor.authorMehdi, Husainen_US
dc.contributor.authorSaxena, Kuldeep Kumaren_US
dc.date.accessioned2024-07-08T12:35:59Z-
dc.date.available2024-07-08T12:35:59Z-
dc.date.issued2023-
dc.identifier.citationMabuwa, S. et al. 2023. Effect of material positioning on Si-rich TIG welded joints of AA6082 and AA8011 by friction stir processing. Journal of Adhesion Science and Technology, 37(17): 2484−2502. [https://doi.org/10.1080/01694243.2022.2142366]en_US
dc.identifier.issn0169-4243-
dc.identifier.issn1568-5616-
dc.identifier.urihttp://hdl.handle.net/11189/9708-
dc.description.abstractThe TIG-welded specimens were friction stir processed (FSPed) to analyze the impact material positioning of the base metals AA8011 and AA6082. The tests included the energy-dispersive Xray spectroscopy (EDS), X-ray diffraction, microstructure, hardness, tensile test and fracture surface analysis. The mean grain size of 24.83 mm was obtained for the TIG welded joint, 8.68 mm for the FSPed joint with AA6082 alloy on the advancing side (A.S), while 11.14 mm was obtained when the AA8011 was positioned on the A.S. In the TIGþFSPed zone, an intricate vortex flow pattern could be seen. The extremely superplastic flow of plasticized material is seen in the mixed flow zone, which results in a tumultuous intercalation pattern. In situ extrusions of different alloys and severe plastic, deformation was induced by stirring tool action. Lamellae structure was generated by moving the plasticized material layer by layer. In this zone, vigorous mixing and penetration of A6082 and AA8011 were observed. The maximum tensile strength and strain rate of the TIG weldment showed a significant increase after friction stir processing from 83.83MPa with a strain rate of 23.79% to 90.09MPa with a tensile strain of 28.04. However, evaluating the FSPed joints, the AA8011-AA6082 specimen had better tensile properties. Moreover, the fracture surface analysis correlated with the tensile tests. The FSPed AA6082-AA8011 joint showed a higher hardness than the AA8011-AA6082 one.en_US
dc.language.isoenen_US
dc.publisherTaylor & Francis: STM, Behavioural Science and Public Health Titlesen_US
dc.relation.ispartofJournal of Adhesion Science and Technologyen_US
dc.subjectMicrostructureen_US
dc.subjectdynamic recrystallisationen_US
dc.subjecttensile propertiesen_US
dc.subjectmicrohardnessen_US
dc.subjectfractographyen_US
dc.titleEffect of material positioning on Si-rich TIG welded joints of AA6082 and AA8011 by friction stir processingen_US
dc.identifier.doihttps://doi.org/10.1080/01694243.2022.2142366-
dc.typeArticleen_US
Appears in Collections:Eng - Journal articles (DHET subsidised)
Files in This Item:
File Description SizeFormat 
Effect_material_positioning_Si-rich_TIG.pdf4.61 MBAdobe PDFView/Open
Show simple item record

Page view(s)

91
Last Week
0
Last month
3
checked on Aug 13, 2026

Download(s)

106
checked on Aug 13, 2026

Google ScholarTM

Check

Altmetric


Items in Digital Knowledge are protected by copyright, with all rights reserved, unless otherwise indicated.