Please use this identifier to cite or link to this item: http://hdl.handle.net/11189/9477
DC FieldValueLanguage
dc.contributor.authorHashmi, Abdul Wahaben_US
dc.contributor.authorMehdi, Husainen_US
dc.contributor.authorMabuwa, Sipokazien_US
dc.contributor.authorMsomi, Velaphien_US
dc.contributor.authorMohapatra, Prabhujiten_US
dc.date.accessioned2023-10-12T08:49:50Z-
dc.date.available2023-10-12T08:49:50Z-
dc.date.issued2022-
dc.identifier.citationHashmi, A.W., Mehdi, H., Mabuwa, S. et al. 2022. Influence of FSP parameters on wear and microstructural characterization of dissimilar TIG welded joints with Si-rich filler metal. Silicon, 14(17): 1-15. [https://doi.org/10.1007/s12633-022-01848-8]en_US
dc.identifier.issn1876-990X-
dc.identifier.issn1876-9918-
dc.identifier.urihttp://hdl.handle.net/11189/9477-
dc.description.abstractThe welding process is used to join similar or dissimilar alloys, resulting in severe joint softening, uneven grain structure, and inevitable deficiencies. The friction stir process (FSP) can reduce the grain size and enhance the tensile properties. In this work, the FSP was applied to Si-rich TIG welded joints to enhance the tensile properties and microstructure of the TIG-welded joints by variation of rotational tool speed (TRS), and it was observed that the TIG welding defects (solidification defects, micro-voids, porosity, coarse grain structure) were removed, and the grain size of the TIG weldment was decreased. The coarse eutectic Al13Fe4 and Mg2Si phases were transformed into very small phases in the TIG + FSPed joints. The homogenization of the primary α-Al exists in the TIG welded joints was continuously enhanced as the TRS increased. The processed zone with high TRS (1100 rpm) demonstrated higher tensile strength (102.76 MPa), whereas the TIG weldment using filler ER4043 was employed to have an average tensile strength of 72.14 MPa. The ultrafine grain structure of 5.14 μm was found in the TIG + FSPed weldment with a TRS of 1100 rpm, while the coarse grain size of 20.85 μm was found in the TIG weldment.en_US
dc.language.isoenen_US
dc.publisherSpringer Verlag (Germany)en_US
dc.relation.ispartofSiliconen_US
dc.subjectFriction stir processingen_US
dc.subjectmicrostructureen_US
dc.subjectmicrohardnessen_US
dc.subjecttensile strengthen_US
dc.titleInfluence of FSP parameters on wear and microstructural characterization of dissimilar TIG welded joints with Si-rich filler metalen_US
dc.identifier.doihttps://doi.org/10.1007/s12633-022-01848-8-
dc.typeArticleen_US
Appears in Collections:Eng - Journal articles (DHET subsidised)
Files in This Item:
File Description SizeFormat 
Influence_FSP_Parameters_Wear_Microstructural.pdf20.03 MBAdobe PDFView/Open
Show simple item record

Page view(s)

63
Last Week
0
Last month
5
checked on Aug 13, 2026

Download(s)

75
checked on Aug 13, 2026

Google ScholarTM

Check

Altmetric


Items in Digital Knowledge are protected by copyright, with all rights reserved, unless otherwise indicated.